5/28/2023 0 Comments Factsage download![]() X-ray diffraction results were good consistent with the simulation results. Then, the formula with a slag content of 40wt% was selected and optimized. This is because increasing magnesium can promote the formation of pyroxene. When the slag ratio is above 45wt%, pyroxene is generated more than anorthite. The simulation results indicate that mullite is generated but drastically reduced at the slag ratios of 0–25wt%, and anorthite is the dominant crystalline phase in the slag content of 25wt%-45wt%. In this paper, a series of ceramics with different slag ratios (0–70wt%) were designed, and the software FACTsage was introduced to simulate the formation of crystalline phases. However, the relationship among the initial composition, ceramic microstructure, and macroscopic properties requires further study. ![]() Abstract Using steel slag as a main raw material of ceramics is considered as a high value-added way.